Luran S ECO 777K BC50
Luran® S acrylonitrile styrene acrylate (ASA) polymers feature high surface quality and good impact strength including enhanced colour fastness. The products deliver superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S ECO 777K is considered as the standard injection molding grade within the Luran S portfolio offering a well-balanced property profile. Luran S ECO 777K BC50 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Key Features
- Balanced properties
- Easy processing
- Long-term property retention
- UV resistance
Applications
- Unpainted automotive exterior: radiator grills
- Housings for electrical & electronic devices
- Household applications
- Gardening tools
- Toys, sports & leisure
Industries
-
Grade Version
Please Sign in or Register with INEOS Styrolution to download REACH and other Regulatory Documents
New to INEOS Styrolution? Registration
-
Properties
Properties of Luran S ECO 777K
Property, Test Condition Standard Unit Values Sustainability Properties Carbon Footprint Reduction vs Fossil-Based (3rd party validated) ISO 14044 % 58 Attributed Content of ISCC-certified Bio-Circular Sources (min.) - % 50 Rheological Properties Melt Volume Rate 220 °C/10 kg ISO 1133 cm³/10 min 15 Mechanical Properties Charpy Notched Impact Strength, 23° C ISO 179/1eA kJ/m² 17 Charpy Notched Impact Strength, -30 °C ISO 179/1eA kJ/m² 4 Charpy Unnotched, 23 °C ISO 179/1eU kJ/m² 160 Tensile Modulus ISO 527 MPa 2300 Tensile Stress at Yield, 23 °C ISO 527 MPa 48 Tensile Strain at Yield, 23 °C ISO 527 % 3.3 Nominal Strain at Break, 23 °C ISO 527 % 10 Flexural Modulus, 23 °C ISO 178 MPa 2300 Flexural Strength, 23 °C ISO 178 MPa 70 Hardness, Ball Indentation ISO 2039-1 MPa 80 Thermal Properties Vicat Softening Temperature VST/B/50 (50N, 50 °C/h) ISO 306 °C 97 Heat Deflection Temperature A; (annealed 4 h/80 °C; 1.8 MPa) ISO 75 °C 97 Heat Deflection Temperature B; (annealed 4 h/80 °C; 0.45 MPa) ISO 75 °C 101 Coefficient of Linear Thermal Expansion ISO 11359 10-6/°C 80 - 110 Thermal Conductivity ISO 22007-4 W/(m K) 0.17 Other Properties Density ISO 1183 kg/m³ 1070 Water Absorption, Saturated at 23 °C ISO 62 % 1.65 Moisture Absorption, Equilibrium 23 °C/50% RH ISO 62 % 0.35 Burning rate (US-FMVSS), 2.0 mm ISO 3795 mm/min 30 UL94 rating at 1.5 mm thickness IEC 60695-11-10 - HB Processing Melt Temperature Range ISO 294 °C 240 - 280 Mold Temperature Range ISO 294 °C 40 - 80 Drying Temperature - °C 80 Drying Time - h 2 - 4 Linear Mold Shrinkage ISO 294-4 % 0.4 - 0.7 Typical values for uncolored products
Please note that all processing data stated are only indicative and may vary depending on the individual processing complexities.
Please consult our local sales or technical representatives for details. -
Processing
Processing of Luran S ECO 777K
-
Safety Data Sheet