Styroflex 2G66
The product line Styroflex® comprises thermoplastic elastomers from clear styrene butadiene copolymers (S-TPE), which are more polar than comparable SBS or SEBS grades. The grades provide a very high puncture resistance to foils in multilayer applications and increase as additive the toughness of compounds. They are easy to process and work as modifiers and compatibilizers in many polymers, e.g. polyolefins. For all Styroflex® grades food contact statements are available upon request. Styroflex® 2G66 is suitable for extrusion (blown and cast film) and injection molding and offers a combination of high resilience and toughness with good transparency and process stability. 2G66 is also offered for medical applications and is Gamma, X-ray & ETO sterilizable.
Key Features
- Easy processing
- Well extrudable
- Puncture resistance
- Sterilisable(ETO, NO2, Irradiation)
- Toughness
Applications
- Food contact applications
- Medical devices
- Flexible packaging
- Flexible medical applications, e.g. tubes
- Impact-modified compounds
-
Grade Version
Please Sign in or Register with INEOS Styrolution to download REACH and other Regulatory Documents
New to INEOS Styrolution? Registration
-
Properties
Properties of Styroflex 2G66
Property, Test Condition Standard Unit Values Rheological Properties Melt Flow Rate, 200 °C/5 kg ASTM D 1238 g/10 min 11 Mechanical Properties Tensile Stress at Yield, 23 °C ASTM D 638 psi 450 Tensile Modulus ASTM D 638 psi x 10³ 19 Tensile Modulus (MD) ASTM D 882 psi 25000 Tensile Modulus (TD) ASTM D 882 psi 19000 Elongation at Break (MD) ASTM D 882 % > 500 Elongation at Break (TD) ASTM D 882 % > 500 Flexural Modulus, 23 °C ASTM D 790 psi x 10³ 12 Flexural Stress at 5% Deflection ASTM D 790 psi 392 Hardness, Shore D ASTM D 2240 - 36 Hardness, Shore A ASTM D 2240 - 91 Elemendorf Tear (MD) ASTM D 1922 lbs 1.17 Elemendorf Tear (TD) ASTM D 1922 lbs 1.19 Puncture, Energy at Peak Force ASTM D 3763 in-lb 21.3 Puncture, Total Energy ASTM D 3763 in-lb 30.2 Elongation, Failure ASTM D 638 % > 500 Thermal Properties Vicat Softening Temperature, B/1 ( 120 °C/h, 10N) ASTM D 1525 °F 118 Electrical Properties Volume Resistivity ASTM D 257 - >1013 Surface Resistivity ASTM D 257 - 1015 Optical Properties Refractive Index, Sodium D Line ASTM D 542 - 1.565 Light Transmission at 550 nm ASTM D 1003 % 93 Haze ASTM D 1003 % 1 Other Properties Density (ASTM ) ASTM D 792 g/cm³ 1 Water Shrinkage (100 °C for 30 sec.) - % 0.63 Oxygen Transmission Rate (23 °C/0% RH) ASTM D 3985 cc/100in²/day 5580 Water Vapor Transmission Rate (WVTR) (23 °C/0% to 85% RH gradient) ASTM F1249-06 g/100in²/day 8 - 10 Typical values for uncolored products
Please note that all processing data stated are only indicative and may vary depending on the individual processing complexities.
Please consult our local sales or technical representatives for details. -
Processing
Processing of Styroflex 2G66
-
Safety Data Sheet