Terlux HD 2822
Terlux® HD 2822 is a standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well known in SAN molding compositions. Food contact statements are available on request.
Key Features
- Chemical resistance
- Impact strength
- Sterilisable(ETO,NO2, Irradiation)
- Transparency
Applications
- Medical devices
- Medical diagnostic equipment
-
Grade Version
Bitte melden Sie sich an oder registrieren Sie sich bei INEOS Styrolution um REACH oder Regulatorische Dokumente herunterladen zu können
Neu bei INEOS Styrolution? Registrieren Kundenregistrierung
-
Properties
Properties of Terlux HD 2822
Property, Test Condition Standard Unit Values Rheological Properties Melt Volume Rate 220 °C/10 kg ISO 1133 cm³/10 min 2 Mechanical Properties Charpy Notched Impact Strength, 23° C ISO 179/1eA kJ/m² 5 Charpy Notched Impact Strength, -30 °C ISO 179/1eA kJ/m² 2 Charpy Unnotched, 23 °C ISO 179/1eU kJ/m² 120 Charpy Unnotched, -30 °C ISO 179/1eU kJ/m² 80 Tensile Modulus ISO 527 MPa 2000 Tensile Stress at Yield, 23 °C ISO 527 MPa 48 Tensile Strain at Yield, 23 °C ISO 527 % 4 Nominal Strain at Break, 23 °C ISO 527 % 12 Flexural Modulus, 23 °C ISO 178 MPa 2000 Flexural Strength, 23 °C ISO 178 MPa 70 Hardness, Ball Indentation ISO 2039-1 MPa 70 Thermal Properties Vicat Softening Temperature VST/B/50 (50N, 50 °C/h) ISO 306 °C 93 Vicat Softening Temperature, VST/A/50 (10N, 50 °C/h) ISO 306 °C 105 Heat Deflection Temperature A; (annealed 4 h/80 °C; 1.8 MPa) ISO 75 °C 90 Heat Deflection Temperature B; (annealed 4 h/80 °C; 0.45 MPa) ISO 75 °C 94 Coefficient of Linear Thermal Expansion ISO 11359 10-6/°C 80 - 110 Thermal Conductivity ISO 22007-4 W/(m K) 0,17 Optical Properties Refractive Index, Sodium D Line ISO 489 - 1,54 Haze ASTM D 1003 % < 3 Light Transmission at 550 nm ASTM D 1003 % 89 Other Properties Density ISO 1183 kg/m³ 1080 Water Absorption, Saturated at 23 °C ISO 62 % 0,7 Processing Linear Mold Shrinkage ISO 294-4 % 0,4 - 0,7 Melt Temperature Range ISO 294 °C 230 - 260 Mold Temperature Range ISO 294 °C 50 - 75 Drying Temperature - °C 70 Drying Time - h 2 Typical values for uncolored products
Please note that all processing data stated are only indicative and may vary depending on the individual processing complexities.
Please consult our local sales or technical representatives for details. -
Processing
Processing of Terlux HD 2822
-
Safety Data Sheet